4210
Spiderbond
3506.9190
Availability: | |
---|---|
Quantity: | |
Polyolefin Web Adhesive
4210
Description
Spiderbond 4210 web adhesive is a nonwoven form hot melt adhesive produced based on polyolefin. Web adhesives handle like a fabric facilitating both intermittent and continuous processes. The PO web is available in a range of basis weights from 3 grams to 150 grams per square meter.
4210 web adhesive is based upon modified polyolefin polymer. This product offer good resistance to repeated home launderings, bond to a wide variety of textiles, foams, paper, leather, polymer and plastic materials, etc.
Advantages
Web pattern produces porous bonds.
VOC free adhesive in easy handle web form.
Strong bonding strength and good anti-washing performance.
Material properties:
Property | Detail or Method | Specification |
Appearance | Bye eye | White web |
Base | Polyolefin | |
Basis Weight Range | g/m² | 3-150, tolerance ±10% |
Width | cm | Max 360, tolerance 0-10mm |
Melting range | DSC, °C | 95-105 |
Recommend Application Temperature | °C | 130-150 |
Packaging:
4210 web adhesives are sold in roll form, pack in carton.
For further packaging details please contact our salesperson.
Shelf Life:
4210 should be shipped and stored at temperatures below 50°C. The shelf life of 4210 is one year under these conditions.
Directions for Using:
4210 web can be activated with any of the following techniques: electric fusing press, heated rolls, heated air, radiant heat, or steam press. Dry heat activation recommend above 95°C.
Reactivation time is dependent upon technique, temperature, pressure, substrates, and adhesive thickness, but would typically be in a temperature of 130°C~150°C with pressure of 1~3MPa to the adherend, andmaintain the pressure for 10~20 seconds to complete the bonding.
The surface of the adherend should be as clean and dry as possible, free of solvents and grease. Lower adherent surface temperatures or ambient temperatures will cause early adhesive coagulation, reducing open time and even causing adhesive shedding. Preheat the adherend if necessary.
Health & Safety Precautions
The Safety Data Sheet should be consulted for proper handling, clean up and spill containment before use. Keep containers covered to minimize contamination.
Our Service:
1. Samples send to you free of charge.
2. Delivery on time, quality according to customer request.
3. OEM, ODM is welcome.
4. Support small wholesale, retails, Any inquires will be replied within 24 hours.
Polyolefin Web Adhesive
4210
Description
Spiderbond 4210 web adhesive is a nonwoven form hot melt adhesive produced based on polyolefin. Web adhesives handle like a fabric facilitating both intermittent and continuous processes. The PO web is available in a range of basis weights from 3 grams to 150 grams per square meter.
4210 web adhesive is based upon modified polyolefin polymer. This product offer good resistance to repeated home launderings, bond to a wide variety of textiles, foams, paper, leather, polymer and plastic materials, etc.
Advantages
Web pattern produces porous bonds.
VOC free adhesive in easy handle web form.
Strong bonding strength and good anti-washing performance.
Material properties:
Property | Detail or Method | Specification |
Appearance | Bye eye | White web |
Base | Polyolefin | |
Basis Weight Range | g/m² | 3-150, tolerance ±10% |
Width | cm | Max 360, tolerance 0-10mm |
Melting range | DSC, °C | 95-105 |
Recommend Application Temperature | °C | 130-150 |
Packaging:
4210 web adhesives are sold in roll form, pack in carton.
For further packaging details please contact our salesperson.
Shelf Life:
4210 should be shipped and stored at temperatures below 50°C. The shelf life of 4210 is one year under these conditions.
Directions for Using:
4210 web can be activated with any of the following techniques: electric fusing press, heated rolls, heated air, radiant heat, or steam press. Dry heat activation recommend above 95°C.
Reactivation time is dependent upon technique, temperature, pressure, substrates, and adhesive thickness, but would typically be in a temperature of 130°C~150°C with pressure of 1~3MPa to the adherend, andmaintain the pressure for 10~20 seconds to complete the bonding.
The surface of the adherend should be as clean and dry as possible, free of solvents and grease. Lower adherent surface temperatures or ambient temperatures will cause early adhesive coagulation, reducing open time and even causing adhesive shedding. Preheat the adherend if necessary.
Health & Safety Precautions
The Safety Data Sheet should be consulted for proper handling, clean up and spill containment before use. Keep containers covered to minimize contamination.
Our Service:
1. Samples send to you free of charge.
2. Delivery on time, quality according to customer request.
3. OEM, ODM is welcome.
4. Support small wholesale, retails, Any inquires will be replied within 24 hours.